4J36 (Invar), oo sidoo kale loo yaqaanno guud ahaan FeNi36 (64FeNi gudaha Mareykanka), waa daawaha nikkel-birta oo caan ku ah iskudarkeeda hoose ee ballaarinta kulaylka (CTE ama α).


  • Qaabka NO.:Invar
  • OEM:Haa
  • Gobolka:Jilicsan 1/2 adag T- adag
  • Koodhka HS:74099000
  • Asal ahaan:Shiinaha
  • Cufnaanta:8.1
  • Faahfaahinta Alaabta

    FAQ

    Tags Product

    4J36 (Invar) waxa loo adeegsadaa halka loo baahan yahay xasilooni cabbir sare, sida qalabyada saxda ah, saacadaha, cabbiraadaha seismic ee gurguurta, maaskarada hadhka telefishinka, matoorada matoorada, iyo saacadaha antimagnetic.Sahanka dhulka, marka heerka koowaad (sax-sare) la rabo in la sameeyo heerka sareynta, shaqaalaha Heerka (usha heerka) ee la isticmaalo ayaa laga sameeyayInvar, halkii laga heli lahaa alwaax, fiberglass, ama biraha kale.Invar struts ayaa loo adeegsaday qaar ka mid ah pistons si loo xaddido fidinta kulaylka ee gudaha dhululubadahooda.

    4J36 waxay isticmaashaa alxanka oxyacetylene, alxanka korantada, alxanka iyo hababka kale ee alxanka.Maaddaama isku-dhafka balaadhinta iyo ka kooban kiimikada ee daawaha ay la xiriirto waa in laga fogaadaa sababtoo ah alxanka ayaa keenaya isbeddel ku yimaada halabuurka daawaha, waxaa la doorbidaa in la isticmaalo biraha alxanka alxanka Argon arc oo doorbidaya ka kooban 0.5% ilaa 1.5% titanium, si yaree porosity alxanka iyo dildilaaca.

    Halabuurka caadiga ah%

    Ni 35-37.0 Fe Bal. Co - Si ≤0.3
    Mo - Cu - Cr - Mn 0.2 ~ 0.6
    C ≤0.05 P ≤0.02 S ≤0.02

    Isku-dhafka ballaarinta

    θ/ºC α1/10-6ºC-1 θ/ºC α1/10-6ºC-1
    20 ~ -60 1.8 20 ~ 250 3.6
    20 ~ -40 1.8 20-300 5.2
    20 ~ -20 1.6 20 ~ 350 6.5
    20 ~-0 1.6 20 ~ 400 7.8
    20 ~ 50 1.1 20 ~ 450 8.9
    20 ~ 100 1.4 20-500 9.7
    20 ~ 150 1.9 20 ~ 550 10.4
    20-200 2.5 20 ~ 600 11.0

     

    Tilmaamaha Jireed ee caadiga ah

    Cufnaanta (g/cm3) 8.1
    Iska caabin koronto oo ah 20ºC(OMmm2/m) 0.78
    Qodobka heerkulka iska caabbinta (20ºC ~ 200ºC)X10-6/ºC 3.7 ~ 3.9
    Dhaqdhaqaaqa kulaylka, λ/ W/(m*ºC) 11
    Dhibicda Curie Tc/ºC 230
    Modulus Elastic, E/Gpa 144

     

    Habka daaweynta kulaylka
    Annealing si loo yareeyo walbahaarka Kuleylka ilaa 530 ~ 550ºC oo qabo 1 ~ 2 saacadood.Qabow
    nuugista Si loo baabi'iyo qallafsanaanta, kaas oo lagu soo saaro qabow-duuban, habka sawirka qabow.Annealing waxay u baahan tahay kuleyl ilaa 830 ~ 880ºC meel faaruq ah, qabo 30 daqiiqo.
    Habka xasilinta
    1. Warbaahinta ilaalinta oo kuleyl ilaa 830ºC, qabo 20min.~ 1 saac
    2. Cadaadiska ka dhashay deminta, kuleyl ilaa 315ºC, qabo 1 ~ 4h.
    Ka taxadaritaan
    1. Laguma adkeyn karo daawaynta kulaylka
    2. Daawaynta dusha sare waxay noqon kartaa ciid-qarxinta, dhalaalid ama qajaar.
    3. Alloy waxaa loo isticmaali karaa 25% hydrochloric acid xalinta 70ºC si loo nadiifiyo oogada oksaydheysan

    Guryaha makaanikada ee caadiga ah

    Xoogga Jilicsan Dheeraynta
    Mpa %
    641 14
    689 9
    731 8

    Qodobka heerkulka iska caabinta

    Kala duwanaanta heerkulka,ºC 20 ~ 50 20 ~ 100 20-200 20-300 20 ~ 400
    aR/ 103 *ºC 1.8 1.7 1.4 1.2 1.0