Cronix 70 waxaa loo isticmaalaa kuleyliyaha korontada u adkaysta daxalka ee foornada warshadaha leh jawi yareeya. Cronix 70 aad ayuu u adkaystaa oksaydhka hawada. Laguma talinayo in loo isticmaalo walxaha kululaynta ee dahaarka leh ee MgO, ama isticmaalka iyadoo la adeegsanayo jawi nitrogen ama kaarburizing ah.
| Fasal | Ni80Cr20 | Ni70Cr30 | Ni60Cr23 | Ni60Cr15 | Ni35Cr20 | Karma | Evanohm | |
| Halabuurka magacaaban% | Ni | Bal | Bal | 58.0-63.0 | 55.0-61.0 | 34.0-37.0 | Bal | Bal |
| Cr | 20.0-23.0 | 28.0-31.0 | 21.0-25.0 | 15.0-18.0 | 18.0-21.0 | 19.0-21.5 | 19.0-21.5 | |
| Fe | ≦1.0 | ≦1.0 | Bal | Bal | Bal | 2.0-3.0 | - | |
| Al1.0-1.7 Ti 0.3-0.5 | Al2.7-3.2 Mn0.5-1.5 | Al2.7-3.2 Cu2.0-3.0 Mn0.5-1.5 | ||||||
| Heerkulka ugu badan ee hawlgalka (°C) | 1200 | 1250 | 1150 | 1150 | 1100 | 300 | 400 | |
| Adkeysiga (Ω/cmf, 20℃) | 1.09 | 1.18 | 1.21 | 1.11 | 1.04 | 1.33 | 1.33 | |
| Adkeysiga (uΩ/m, 60°F) | 655 | 704 | 727 | 668 | 626 | 800 | 800 | |
| Cufnaanta (g/cm³) | 8.4 | 8.1 | 8.4 | 8.2 | 7.9 | 8.1 | 8.1 | |
| Qaboojinta Kulaylka (KJ/m·h·℃) | 60.3 | 45.2 | 45.2 | 45.2 | 43.8 | 46.0 | 46.0 | |
| Isugeynta Ballaarinta Toosan(×10¯6/℃) 20-1000℃) | 18.0 | 17.0 | 17.0 | 17.0 | 19.0 | - | - | |
| Barta Dhalmada (℃) | 1400 | 1380 | 1370 | 1390 | 1390 | 1400 | 1400 | |
| Adkaanta (Hv) | 180 | 185 | 185 | 180 | 180 | 180 | 180 | |
| Xoog Laab Laab (N/mm)2) | 750 | 875 | 800 | 750 | 750 | 780 | 780 | |
| Kordhinta (%) | ≥20 | ≥20 | ≥20 | ≥20 | ≥20 | 10-20 | 10-20 | |
| Qaab-dhismeedka Micrographic | austenit | austenit | austenit | austenit | austenit | austenit | austenit | |
| Hantida Magnetic-ga | Aan ahayn | Aan ahayn | Aan ahayn | Si yar | Aan ahayn | Aan ahayn | Aan ahayn | |
| Nolosha Degdegga ah (h/℃) | ≥81/1200 | ≥50/1250 | ≥81/1200 | ≥81/1200 | ≥81/1200 | - | - | |