Darajo | CuNi1 | CuNi2 | CuNi6 | CuNi8 | CuNi10 | CuNi14 | CuNi19 | CuNi23 | CuNi30 |
Heerkulka ugu sarreeya (℃) | 200 | 200 | 220 | 250 | 250 | 300 | 300 | 300 | 350 |
Cufnaanta (g/cm3) | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 |
Iska caabin 20℃(200Cμ. m) | 0.03 ± 10% | 0.05± 10% | 0.10± 10% | 0.12± 10% | 0.15± 10% | 0.20± 5% | 0.25± 5% | 0.30± 5% | 0.35 ± 5% |
Isku-dhafka heerkulka x10-6/℃(20-600℃) | <100 | <120 | <60 | <57 | <50 | <38 | <25 | <16 | <10 |
Xoog xajin (Mpa) | >210 | >220 | >250 | >270 | >290 | >310 | >340 | >350 | >400 |
Kordhinta markay dillaacdo (%) | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 | >25 |
Barta fusing (℃) | 1085 | 1090 | 1095 | 1097 | 1100 | 1115 | 1135 | 1150 | 1170 |
P-copper heerkulbeegyo koronto (μV/℃) (0-100 ℃) | -8 | -12 | -18 | -22 | -25 | -28 | -32 | -34 | -37 |