| Magacaabista | 1J85 |
| Heerka u dhigma | GB /T 32286.1-2015 |
| Calaamadda | Joogto Magnetic Sare leh oo leh Nickel-Iron Alloy |
| Sharaxaad | Habka Daaweynta Kulaylka ee lagu taliyay: * Heerkulka Kululaynta: 1100-1200°C * Waqtiga Qoynta: 3-6 saacadood * Habka Qaboojinta: Qabooji 100-200°C/saacaddii ilaa 500-600°C, ka dibna qabooji heerkul aan ka yarayn 400°C/saacaddii ilaa heerkul ka hooseeya 300°C ka hor inta aan la saarin. Cabbirrada Aasaasiga ah ee Jirka: |
| Cufnaanta | 8.75 g/cm3 |
| Qaybaha Kiimikada | |||||||||
| Qaybaha | C | Si | Mn | P | S | Ni | Cu | Mo | Wax badan |
| Ugu badnaan | 0.03 | 0.3 | 0.6 | 0.02 | 0.02 | 81 | 0.2 | 5.2 | Dheelitirka Fe |
| Ugu yaraan | - | 0.15 | 0.3 | - | - | 79 | - | 4.8 | |