Magaca guud:1Cr13Al4, Alkrothal 14, Alloy 750, Alferon 902, Alchrome 750, Resistohm 125, Aluchrom W, 750 Alloy, Stablohm 750.
TANKII 125 waa aluminium bir-chromium-aluminium ah (FeCrAl alloy) oo lagu garto waxqabadka xasilloon, Anti-oxidation, iska caabbinta daxalka, xasilloonida heerkulka sare, awoodda gariiradda samaynta heer sare ah, Labis iyo xaalad dusha qurux badan oo aan dhibco lahayn.Waxay ku habboon tahay in loo isticmaalo at heerkulka ilaa 950 ° C.
Codsiyada caadiga ah ee TANKII125 waxaa loo isticmaalaa gawaarida korantada, naaftada naaftada, gaari metro ah iyo baabuur dhaqaaqa xawaaraha sare iwm nidaamka bireega caabiyaha, mashiinka karinta dhoobada korontada, foornada warshadaha.
Halabuurka caadiga ah%
C | P | S | Mn | Si | Cr | Ni | Al | Fe | Mid kale |
Max | |||||||||
0.12 | 0.025 | 0.025 | 0.70 | ugu badnaan 1.0 | 12.0-15.0 | ugu badnaan 0.60 | 4.0 ~ 6.0 | Bal. | - |
Guryaha Makaanikada ee caadiga ah (1.0mm)
Xoog soo saar | Xoogga Jilicsan | Dheeraynta |
Mpa | Mpa | % |
455 | 630 | 22 |
Tilmaamaha Jireed ee caadiga ah
Cufnaanta (g/cm3) | 7.40 |
Iska caabin koronto oo ah 20ºC (ohm mm2/m) | 1.25 |
Isku-dheellitirnaanta hab-dhaqanka ee 20ºC (WmK) | 15 |
Isku-dhafka ballaarinta kulaylka
Heerkulka | Isku-dhafka Balaadhinta kulaylka x10-6/ºC |
20ºC-1000ºC | 15.4 |
Awood kuleyl gaar ah
Heerkulka | 20ºC |
J/gK | 0.49 |
Barta dhalaalka (ºC) | 1450 |
Heerkulka hawada ee joogtada ah ee ugu badan (ºC) | 950 |
Guryaha magnetic | aan magnet ahayn |
Falanqaynta Magacaaban
Heerkulka shaqada ee joogtada ah ee ugu badan: 1250ºC.
Heerkulka dhalaalka: 1450ºC
Iska caabin koronto: 1.25 ohm mm2/m
Si aad ah ayaa loo isticmaalay sida walxaha kuleyliyaha ee foornooyinka warshadaha iyo kilnnada korontada.
Wuxu leeyahay awood ka kulul marka loo eego Alloys-ka Tofet laakiin barta dhalaalka oo aad uga sarreeya.