Halabuurka boqolleyda:
Al | Cr | Fe | Mn | C | Si | Ni | Cu | Ti | Mid kale | Curiyayaasha dhulka naadir |
4.6-5.8 | 14.5-15.5 | Saldhig | Max0.7 | ilaa 0.05 | ilaa 0.6 | ilaa 0.6 | … | ilaa 0.6 | Zr≤0.3 | … |
Silig iska caabinta:
1) Birta chrome aluminium silig
CrAl 14-4, CrAl 15-5, CrAl 20-5, CrAl 25-5, iwm.
2) Nichrome Wire
NiCr 80/20, NiCr 70/30, NiCr 60/15, NiCr 35/20
3)Nickel Copper Alloy Wire
Alloy 30, Alloy 60, Alloy 90, Constantan Wire
Faahfaahin dheeraad ah, pls booqo boggayaga ama email noogu soo dir
QAABKA:
1Cr13Al4 | 0.03-12.0 | 1.25±0.08 | 588-735 | >16 | >6 | 950 | >10000 |
0Cr15Al5 | 1.25±0.08 | 588-735 | >16 | >6 | 1000 | >10000 | |
0Cr25Al5 | 1.42± 0.07 | 634-784 | >12 | >5 | 1300 | >8000 | |
0Cr23Al5 | 1.35±0.06 | 634-784 | >12 | >5 | 1250 | >8000 | |
0Cr21Al6 | 1.42± 0.07 | 634-784 | >12 | >5 | 1300 | >8000 | |
1Cr20Al3 | 1.23±0.06 | 634-784 | >12 | >5 | 1100 | >8000 | |
0Cr21Al6Nb | 1.45 ± 0.07 | 634-784 | >12 | >5 | 1350 | >8000 | |
0Cr27Al7Mo2 | 0.03-12.0 | 1.53±0.07 | 686-784 | >12 | >5 | 1400 | >8000 |
ku haboon:
Fecrak noo daawaha ku habboon oo leh iska caabin dhab ah oo gaar ah oo xad-dhaaf ah (1.20-1.30 ohm-mm2/m) kaas oo isku dara caabbinta kulaylka ilaa 1450C waxaana lagu andacoonayaa in laga maarmi karo heerkulka ugu sarreeya . Waxay leedahay iska caabin daxalka qumman hawada, gudaha argon, vacuum, oxidizing, baaruud-ku jira iyo deegaanka carboniferous.Waxay muujinaysaa ma aha mid aad u sarreeya cufnaanta qaraabo (7.2g / cm3), laakiin waxa ay leedahay xad wax soo saarka weyn.
Cr15Al5 Eurofechral
maaddo | darajo | Magaca UNS | DIN | Cufnaanta | ASTM |
saxaro | 1.4725 | K 92500 | 17470kii | 7.4 | B 603-1 |
Codsiyada ugu muhiimsan:foornos, walxaha iska caabinta, foornooyinka kulaylka sareeyo, walxaha kululaynta tuubada warshadaha iyo kuleyliyeyaasha.
Astaamaha Makaanikada T°20°C
Tirada qaansooyinka | Kordhinta boqolkiiba |
:5 jeer | :16% |
Astaamaha Jirka T°20°C
Adag | Cufnaanta | Culayska jabinaya | Heerkulka shaqada ee ugu badan 850C | Iska caabin koronto | Magnetism | Dhibcaha dhalaalinta (°C) |
200-260 HB | 7.1g/cm3 | 637-784m/pa | 1.30 ohn-mm2/m | Magnetik | 1400 °C |