Tankii CuNi44 waxay bixisaa iska caabin koronto oo sarreeya iyo heerkulka iska caabbinta oo aad u hooseeya (TCR). Sababtoo ah TCR-ga hooseeya, waxay ka heleysaa isticmaalka caabiyeyaasha saxda ah ee dhaawaca silig-dhaawaca kuwaas oo shaqeyn kara ilaa 400 ° C (750 ° F). Alloyskani waxa kale oo uu awood u leeyahay in uu horumariyo xoog koronto oo joogto ah marka lagu daro naxaas. Gurigan wuxuu u oggolaanayaa in loo isticmaalo kuleylaha kuleylaha, kordhinta kuleylaha iyo magdhowga hogaanka. Si fudud ayaa loo iibiyaa, loo alxanayaa,
Alloy | Workstoff Nr | Magacaabista UNS | DIN |
---|---|---|---|
CuNi44 | 2.0842 | C72150 | 17644kii |
Alloy | Ni | Mn | Fe | Cu |
---|---|---|---|---|
CuNi44 | Min 43.0 | ugu badnaan 1.0 | ugu badnaan 1.0 | Dheelitiran |
Alloy | Cufnaanta | Iska caabin gaar ah (Kacsiga Korontada) | Kuleylka toosan Balaadhinta Coeff. b/w 20 - 100°C | Heerkulka Coeff ee iska caabinta b/w 20 - 100°C | Ugu badnaan Heerkulka Shaqada ee Element | |
---|---|---|---|---|---|---|
g/cm³ | µΩ-cm | 10-6/°C | ppm/°C | °C | ||
CuNi44 | 8.90 | 49.0 | 14.0 | Heerka | ± 60 | 600 |
Gaar ah | ±20 |