| Nikkel | 23 | Manganese | 0.5 |
| Copper | Bal. |
| Xoog soo saar | Xoogga Jilicsan | Dheeraynta |
| Mpa | Mpa | % |
| 170 | 350 | 25 |
| Cufnaanta (g/cm3) | 8.9 |
| Iska caabin koronto oo ah 20ºC (Ωmm2/m) | 0.30 |
| Qodobka heerkulka iska caabbinta (20ºC ~ 600ºC)X10-5/ºC | <16 |
| Isku-dheellitirnaanta hab-dhaqanka ee 20ºC (WmK) | 33 |
| EMF vs Cu (μV/ºC )(0~100ºC) | -34 |
| Isku-dhafka ballaarinta kulaylka | |
| Heerkulka | Balaadhinta kulaylka x10-6/K |
| 20ºC-400ºC | 17.5 |
| Awood kuleyl gaar ah | |
| Heerkulka | 20ºC |
| J/gK | 0.380 |
| Barta dhalaalka (ºC) | 1150 |
| Heerkulka hawada ee joogtada ah ee ugu badan (ºC) | 300 |
| Guryaha magnetic | aan magnet ahayn |
Waxqabadka iska caabinta daxalka
| Alloys | Ku shaqaynta jawiga 20ºC | Ku shaqeynta heerkulka ugu sarreeya 200ºC | |||||
| Hawo iyo ogsijiin ayaa ka kooban gaasaska | gaasaska leh Nitrogen | gaasaska leh baaruud oksidability | gaasaska leh baaruud dhimis | carburization | |||
| Alloy 180 | wanaagsan | guud | guud | guud | xun | wanaagsan | |